Grinding Wheel Selection for Surface Grinders: A Practical Chart
Which grinding wheel for die steel, hardened steel, aluminium, carbide and cast iron — grit, grade, bond and wheel size by material.
Start from the material, not the wheel catalogue
Wheel choice is decided by three properties of the work: hardness, thermal sensitivity and whether it is ferrous. Everything else — grit number, grade letter, bond type — follows from those.
| Work material | Grit | Grade | Bond | Typical depth / pass |
|---|---|---|---|---|
| Pre-hardened die steel (28–34 HRC) | 46–60 | J–K | Vitrified | 0.3–0.5 mm |
| Hardened tool steel (50–62 HRC) | 60–80 | H–J | Vitrified | 0.1–0.25 mm |
| Cast iron | 46–60 | J | Vitrified | 0.4–0.6 mm |
| Aluminium | 24–46 | H–I | Open, soft | 0.5–1.0 mm |
| Carbide | Diamond 100–150 | Resin | Resin | 0.01–0.02 mm |
| Ceramics / glass | Diamond 80–120 | Resin | Resin / metal | 0.02–0.05 mm |
White vs pink vs micro-crystalline alumina
White alumina is the general-purpose choice for die steel. Pink alumina holds its edge better on hardened work above 50 HRC. Micro-crystalline alumina (such as SG-type grit) lasts two to three times longer on hard work but costs more — worth it only if the machine runs production hours.
Signs the wheel is wrong
- Glazing (shiny surface, no spark, burn marks): grade too hard or wheel too fine. Move one grade softer.
- Rapid breakdown (wheel loses shape, taper appears): grade too soft. Move one grade harder.
- Chatter marks: wheel out of balance, or wheel too hard and loading.
- Loading on aluminium: wheel too dense or coolant delivery too poor — use a coarse open wheel and more flow.
Wheel speed and maximum RPM
Never exceed the RPM printed on the wheel. A 350 mm wheel designed for 1,450 rpm must not run on a 2,850 rpm spindle — the burst risk is real and the guard is not designed for it.
Need a machine recommendation for this job? Send the drawing and tolerance to our application engineers — reply within 24 hours.