Silicon Nitride Grinding

Materials · topic notes

Grinding silicon nitride: wheel grade, depth of cut, coolant and the flatness that is realistic on a surface grinder. no linked items yet filed under this topic.

What Silicon Nitride Grinding covers

Thin or long parts move under the wheel no matter what the material is, so clamping and stress relief belong in this topic too.

How to specify silicon nitride grinding

  • Hardened tool steel above 55 HRC wants a softer grade and a shallower depth of cut
  • Aluminium loads a vitrified wheel: use a coarser grit, more coolant, or a coated abrasive
  • Stainless steels work-harden, so keep the wheel cutting rather than rubbing
  • Cemented carbide and ceramics need diamond, and the machine needs to be stiff enough to use it

Where silicon nitride grinding goes wrong

The test: grind one pass at the intended depth on a sample, then look for temper colours, cracks under a magnifier, and check Ra. Those three signs tell you which of the three variables to change.

Machines and reading for silicon nitride grinding

Topics in this vocabulary point to a machine line rather than to a single offer, so the answer stays useful when the model range changes. For silicon nitride grinding the closest line is precision rotary table grinders; the selection guide and the accuracy notes cover the neighbouring questions.

Products

Machines filed under this topic, plus the closest models from the line it belongs to.

HZ-RT400 Rotary Table Surface Grinder (ø400 mm)

HZ-RT400 Rotary Table Surface Grinder (ø400 mm)

ø400 mm rotary table grinder with vertical spindle — flat rings and discs in one continuous pass.
Details
HZ-RT600 Rotary Table Surface Grinder (ø600 mm)

HZ-RT600 Rotary Table Surface Grinder (ø600 mm)

ø600 mm rotary grinder with 5.5 kW spindle — larger rings and discs with high stock removal.
Details
HZ-RT800 Rotary Table Surface Grinder (ø800 mm)

HZ-RT800 Rotary Table Surface Grinder (ø800 mm)

ø800 mm rotary grinder with 7.5 kW spindle and automatic cycle for heavy rings.
Details

Blog Articles

Cases & Solutions

Questions about Silicon Nitride Grinding

Why does my part burn on the last pass?

Usually a glazed wheel plus a spark-out that is too short, so the wheel rubs instead of cutting. Redress, add coolant flow, and keep a light finishing depth of cut.

Which wheel for hardened steel above 55 HRC?

A softer vitrified grade with 46–60 grit, dressed frequently, at a reduced depth of cut, and with coolant aimed at the contact arc.

Related topics

← Browse all topics  ·  Ask an engineer about this topic