Segment Wheel

Wheels & Coolant · topic notes

Choosing and maintaining a segment wheel: what it changes in the cut and the signs it needs replacing. no linked items yet filed under this topic.

What Segment Wheel covers

Wheel and coolant are where surface finish is actually made; the machine only has to hold the wheel in the right place.

How to specify segment wheel

  • A 400 mm wheel on a 7.5 kW spindle wants a softer grade than the same wheel on 15 kW
  • Concentration matters on diamond and CBN wheels; check the bond, not only the grit
  • Magnetic separators and paper filters remove different particle sizes — most shops need both
  • Coolant concentration below 5% invites rust and above 10% invites skin trouble

Where segment wheel goes wrong

Burn marks and a glazed wheel are the same fault seen from two sides: redress, then check coolant flow and concentration before changing the wheel.

Machines and reading for segment wheel

Topics in this vocabulary point to a machine line rather than to a single offer, so the answer stays useful when the model range changes. For segment wheel the closest line is vertical spindle surface grinders; the selection guide and the accuracy notes cover the neighbouring questions.

Products

Machines filed under this topic, plus the closest models from the line it belongs to.

PSG-V500 Vertical Spindle Surface Grinder (500 × 300 mm)

PSG-V500 Vertical Spindle Surface Grinder (500 × 300 mm)

Cup-wheel vertical spindle grinder that flats a full face in one pass — fast stock removal with no warp.
Details
PSG-V700 Vertical Spindle Surface Grinder (700 × 400 mm)

PSG-V700 Vertical Spindle Surface Grinder (700 × 400 mm)

700 × 400 mm vertical spindle grinder with 7.5 kW spindle for heavier plates.
Details
PSG-V900 Vertical Spindle Surface Grinder (900 × 500 mm)

PSG-V900 Vertical Spindle Surface Grinder (900 × 500 mm)

900 × 500 mm vertical spindle grinder with 11 kW spindle and automatic cycle.
Details

Blog Articles

Cases & Solutions

Questions about Segment Wheel

Which wheel grit should I start with?

60 grit on a vitrified bond covers most die and mould work; move to 46 for stock removal and 120 when the drawing asks for a fine finish.

How often should the wheel be dressed?

Every 20–30 minutes of cutting on steel, and immediately before any finishing pass. A glazed wheel raises the temperature, which is the start of burn and chatter.

Related topics

← Browse all topics  ·  Ask an engineer about this topic
WhatsApp