Plastic Mould Steel Grinding

Materials · topic notes

Grinding plastic mould steel: wheel grade, depth of cut, coolant and the flatness that is realistic on a surface grinder. no linked items yet filed under this topic.

What Plastic Mould Steel Grinding covers

Heat treatment state matters as much as the alloy: the same steel at 45 HRC and 58 HRC grinds differently.

How to specify plastic mould steel grinding

  • Burn is a coolant and dwell problem before it is a wheel problem
  • Pre-hardened plates often need stress relief before grinding, not after
  • Cast iron grinds freely but the graphite in the coolant will stain the next job

Where plastic mould steel grinding goes wrong

The test: grind one pass at the intended depth on a sample, then look for temper colours, cracks under a magnifier, and check Ra. Those three signs tell you which of the three variables to change.

Machines and reading for plastic mould steel grinding

Topics in this vocabulary point to a machine line rather than to a single offer, so the answer stays useful when the model range changes. For plastic mould steel grinding the closest line is vertical spindle surface grinders; the selection guide and the accuracy notes cover the neighbouring questions.

Products

Machines filed under this topic, plus the closest models from the line it belongs to.

PSG-V500 Vertical Spindle Surface Grinder (500 × 300 mm)

PSG-V500 Vertical Spindle Surface Grinder (500 × 300 mm)

Cup-wheel vertical spindle grinder that flats a full face in one pass — fast stock removal with no warp.
Details
PSG-V700 Vertical Spindle Surface Grinder (700 × 400 mm)

PSG-V700 Vertical Spindle Surface Grinder (700 × 400 mm)

700 × 400 mm vertical spindle grinder with 7.5 kW spindle for heavier plates.
Details
PSG-V900 Vertical Spindle Surface Grinder (900 × 500 mm)

PSG-V900 Vertical Spindle Surface Grinder (900 × 500 mm)

900 × 500 mm vertical spindle grinder with 11 kW spindle and automatic cycle.
Details

Blog Articles

Cases & Solutions

Questions about Plastic Mould Steel Grinding

Why does my part burn on the last pass?

Usually a glazed wheel plus a spark-out that is too short, so the wheel rubs instead of cutting. Redress, add coolant flow, and keep a light finishing depth of cut.

Which wheel for hardened steel above 55 HRC?

A softer vitrified grade with 46–60 grit, dressed frequently, at a reduced depth of cut, and with coolant aimed at the contact arc.