Grinding hastelloy: wheel grade, depth of cut, coolant and the flatness that is realistic on a surface grinder. no linked items yet filed under this topic.

What Hastelloy Grinding covers

Hard and soft materials fail in opposite ways: hard ones burn and crack, soft ones smear and load the wheel.

How to specify hastelloy grinding

  • Hardened tool steel above 55 HRC wants a softer grade and a shallower depth of cut
  • Aluminium loads a vitrified wheel: use a coarser grit, more coolant, or a coated abrasive
  • Stainless steels work-harden, so keep the wheel cutting rather than rubbing
  • Cemented carbide and ceramics need diamond, and the machine needs to be stiff enough to use it

Where hastelloy grinding goes wrong

The test: grind one pass at the intended depth on a sample, then look for temper colours, cracks under a magnifier, and check Ra. Those three signs tell you which of the three variables to change.

Machines and reading for hastelloy grinding

Topics in this vocabulary point to a machine line rather than to a single offer, so the answer stays useful when the model range changes. For hastelloy grinding the closest line is PLC programmable surface grinders; the selection guide and the accuracy notes cover the neighbouring questions.

Products

Machines filed under this topic, plus the closest models from the line it belongs to.

PSG-5012WMS PLC Programmable Surface Grinder (500 × 125 mm)

PSG-5012WMS PLC Programmable Surface Grinder (500 × 125 mm)

Compact 500 × 125 mm grinder with three-axis PLC control — programmable cycles in a small footprint.
Details
PSG-8020WMS PLC Programmable Surface Grinder (800 × 200 mm)

PSG-8020WMS PLC Programmable Surface Grinder (800 × 200 mm)

800 × 200 mm three-axis PLC grinder with automatic dressing and multi-pass cycles.
Details
PSG-9030WMS PLC Programmable Surface Grinder (900 × 300 mm)

PSG-9030WMS PLC Programmable Surface Grinder (900 × 300 mm)

900 × 300 mm PLC grinder with 350 mm wheel — programmable production on medium die plates.
Details

Blog Articles

Cases & Solutions

Questions about Hastelloy Grinding

Why does my part burn on the last pass?

Usually a glazed wheel plus a spark-out that is too short, so the wheel rubs instead of cutting. Redress, add coolant flow, and keep a light finishing depth of cut.

Which wheel for hardened steel above 55 HRC?

A softer vitrified grade with 46–60 grit, dressed frequently, at a reduced depth of cut, and with coolant aimed at the contact arc.